Sanchem Conversion Coatings Fabtech
Home
»
News
»
Sanchem Conversion Coatings Fabtech
Non-Chromate and Non-Chrome Conversion Coating
Sanchem on Zinc, Aluminum and Magnesium
Paramount Metal Finishing applies Sanchem conversion coatings on zinc, magnesium and aluminum. Sanchem is a RoHS compliant chromate-free conversion coating that leaves an electrically conductive clear to gold protective surface treatment. Sanchem is an excellent preparation of aluminum, magnesium or zinc substrates for paint, powder coating and e-coat as well as adhesives. Sanchem can produce far better coating adhesion comparable to hexavalent chromate conversion coatings.
Sanchem is a high-performance conversion coating that offers:
- Clear or gold RoHS compliant coating
- Chromate free
- Excellent corrosion resistance
- Electrically conductive film on wrought aluminum, aluminum castings, magnesium and zinc as well galvanized steel.
- Excellent pretreatment for paint
- High-temperature applications
- Salt Spray 168 hours on aluminum castings
- Cost-effective coating
- Used in sensitive military and medical applications.
Paramount Metal Finishing applies Sanchem conversion coatings to Zinc, Aluminum, and Magnesium cast or wrought substrates. Paramount Metal Finishing can coat Sanchem treated substrates with various paints, powder coatings and dry-film lubricants.