Zinc Nickel Alloy Plating

High Corrosion Resistant Alternative to Cadmium
AMS 2417 ASTM B841 ASTM F1941

Paramount Metal Finishing offers ZINC NICKEL plating to AMS 2417 and ASTM B841 on large parts up to 9 feet in length. Zinc nickel plating as the name suggests is a co-deposited coating of zinc and nickel.

Zinc Nickel is a high performance finish that offers maximum corrosion resistance especially for components used in severe environments. The zinc and nickel alloying creates a distinctive composition that will corrode at a much slower rate than zinc. The combination of approximately 10-15% nickel and the remainder zinc, can offer up to 10X the protection of traditional zinc plating.

Paramount Metal Finishing Zinc Nickel plating benefits:

  • Maximum corrosion resistance
  • Salt Spray 500+ hours
  • RoHS Compliant
  • Increased part life span
  • Alternative to cadmium and hot dip galvanizing
  • Trivalent, Hexavalent and Black Chromates available
  • Parts up to 9 feet in length

Applications:

  • Oil and Gas
  • Hydraulic Components
  • Railway
  • Agricultural Machinery
  • Automotive Industry
  • Electrical Transmission

Paramount Metal Finishing processes and meets to the following specifications:

  • AMS 2417
  • ASTM B841, ASTM F1941

Paramount Metal Finishing is a specialist in zinc nickel plating and is an integrated coating applicator to ASTM, AMS and Military Specifications. We have capabilities to Plate, Anodize, Hard Coat Anodize, Sanchem, Conversion Coat, Paint, Powder Coat and Dry Film Lube in one location.